Randy McCall on tue 13 mar 07


Anyone used this glaze. I tried it and it ran terribly at Cone 6.
Brushed three coats.


Randy
South Carolina
Pottery Web site

http://members.tripod.com/~McCallJ/index.html

Alisha Clarke on wed 14 mar 07


Randy,
I tried some mid-fire Spectrum glazes a couple of years ago, but they
all had the same problem with running an pitting at cone 6. I believe
they are listed as cone 4-6, but I heard others say they work best at
cone 4 or 5. I gave up on them since I wanted to stay at cone 6. I
also gave up on commercial glazes in general because I like knowing
what is going into the glaze and the ability to modify them to fix
glaze problems like this.
Leesh

On 3/13/07, Randy McCall wrote:
> Anyone used this glaze. I tried it and it ran terribly at Cone 6.
> Brushed three coats.
>
>
> Randy
> South Carolina
> Pottery Web site
>
> http://members.tripod.com/~McCallJ/index.html
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
>


--
~~~~~~~~~~~~~~~~~~~~~~~~~
Alisha Clarke
www.alishaclarke.com