Veena Raghavan on sun 11 mar 07


Mel, They look scrumptious! So look forward to seeing the pieces you bring to
NCECA.

Veena


n a message dated 3/11/2007 8:46:54 PM Eastern Daylight Time,
melpots2@VISI.COM writes:
>
> go to my website.
> clayart page.
> and the images are there.
> i got some wonderful oil spots...really big.
> the new black glaze/saturated with copper/chrom and iron.
> lite coat of copper red over.
>

VeenaRaghavan@cs.com

mel jacobson on sun 11 mar 07


go to my website.
clayart page.
and the images are there.
i got some wonderful oil spots...really big.
the new black glaze/saturated with copper/chrom and iron.
lite coat of copper red over.

the val cushing glaze from dannon was a delight.
the flat glaze with soda ash was crap. otto heino
fell off the pots. has to be really thin.
so.
all in all...very nice firing, with some new images for
me to think about.
i will bring a batch to nceca.
mel

from: mel/minnetonka.mn.usa
website: http://www.visi.com/~melpots/

Clayart page link: http://www.visi.com/~melpots/clayart.html