Jamie Yocono on mon 26 feb 07


I rarely use resist, as one of my instructors got me in the habit of not
using it. Too many things it can contaminate.

But every now and then, I'll need it for a lid or something similar.

I don't remember where I read about it, it might have been in PMI many years
ago. Someone suggested using fabric softener. I've used it ever since. It's
inexpensive, and works fine. The smell is nice, too, although it gets a
little overpowering sometimes. Smells like my laundry
room!

Jamie in Vegas