search  current discussion  categories  kilns & firing - raku 

slip and dee's matt raku glaze

updated fri 9 feb 07

 

Sandi Taylor on wed 7 feb 07


Hello,
Recently, we lost our studio glaze book.We are compiling a new one but =
still need a couple of
items so that it can be completed.I have not been able to find a couple =
of recipes.
I would like to have Dee's Matt Raku Glaze and Val Cushing's White slip =
^10 and the colorants used to get=20
the different colored slips.
All of us at our community college studio would be grateful for any help =
anyone can give us.
Thanks
Sandi Taylor
Manatee Community College
Bradenton,Florida.