search  current discussion  categories  kilns & firing - shelves & furniture 

nitrite bonded shelves

updated sun 21 jan 07

 

Nancy Udell on sat 20 jan 07


Ingleborg,

I would be carful with the ones that didn't appear broken. Mine
appeared to be fine when I unpacked them (I thought) tho now I see
there were some chips around the edges. They even went through a
bisque without a load and seemed fine. I was only when I put weight
on them that they cracked.

I'm not going to use the one (of four) that didn't crack or break in
my firing. I'm sending the whole lot back.

Good luck,

Nancy Udell
Santa Fe, NM