coleman porcelain for raku

updated mon 15 jan 07

 

Rickey Lynn Gans on sun 14 jan 07


I have done raku on several pieces of coleman with excellent results.
The smoothness of the porcelain really brings out details of the glazes
such as a nice crackle or a bright copper. I bisqued to cone 06 first,
and then followed usual raku proceedures. I have loved the results I
have gotten.
Rickey Lynn
Art & Ceramics Teacher
Pueblo Del Sol Middle School
in mostly sunny Phoenix, AZ