beardiepaw on sat 6 jan 07


Thanks for the replies, and the Shimbo site was a big help. As always, =
I appreciate it. As soon as I get the porcelain delivered, I'm going to =
see if I can do it. Hopefully, I'll have some pics to add to my site wit=
h at least ONE crystal on it....maybe....I hope.... Sher Morrow

William & Susan Schran User on sun 7 jan 07


On 1/6/07 1:37 PM, "beardiepaw" wrote:

> Thanks for the replies, and the Shimbo site was a big help. As always, I
> appreciate it. As soon as I get the porcelain delivered, I'm going to see if
> I can do it.

You can do it!

FYI - You don't have to use porcelain for the catch basin. Any stoneware
clay that will fire to the cone you're using will work. Don't waste the
porcelain on something you'll throw away.

--
William "Bill" Schran