fran johnson on thu 7 dec 06


I remember this body from grad school(early 70s). Only
we called it 25 body. When I first set up my studio I
used it at ^4 in an electric kiln. It fired ok, not
vitrified of course, but worked for me. One of the
things I was told was it had a wide firing range.
I never liked working with it- seemed short. I did use
it to make colored clays.
I don't see why it wouldn't work at ^6. Try it and
see.