yellow withiut stains,ravenscrag slip

updated thu 30 nov 06

 

Claudia MacPhee on wed 29 nov 06




  Glad to see someone else is discovering the joys of Ravenscrag slip. It is simple. simple, simple. Where else do you get a really useful  ^6 base with just two items ? Add some oxides and some other 'goodies' and you have lots of room to experiment.  It also works well as a base for layering.

  Our weather has improved by 20 degrees, being only -20 this morning instead of -45 C like two days ago. Still too cold to fire the new wood kiln.....when I do I will see what ravenscrag does at ^10 ( I hope).

  Go see their website, lots of ideas to start.

 