Jacqueline Miller on wed 8 nov 06


Our art center has used Laguna Robins Egg glaze for years with no
problems. The last batch of dipping glaze begins to peel off the
bisque dramatically as soon as it dries. The only way it does not peel
is to have it very, very thin and then it is streaky and not like it
is usually at all. The ceramics director called Laguna but did not get
Jon. The person she spoke to said it must be old (it was bought in
July or Aug '06) and to add CMC which was added with no help. Has
anyone else had this problem? Jon, if you are out there, do you have
any thoughts? Thanks so much,
Jackie

--