cress fe29p kiln

updated thu 9 nov 06

 

Heisler-Schafer, Tamie on wed 8 nov 06


Hello:

I just bought an 20 year old Cress FE29P electric kiln but unfortunately
it came with no manual. When I contacted Cress they said they did not
have any back issues of the manual. So, I'm hoping someone out there
can tell me a few details about firing with this kiln. There are
setting for the firing speed (A, B, C, D - normal to low plus manual),
plus there is a thumbwheel dial which can be set from 1 to 10. I'd
really appreciate it if someone can give me some advice on setting the
dials for bisquing (cone 06) and glazing (cone 6). Thanks very much!
-Tamie=20

Maxwell, Deborah on wed 8 nov 06


Tamie,

It's your lucky day! I have a Cress Kiln Owners Manual that you may
have. Email me off line with your address and I will pop it in the mail!
I was going to purchase a Cress kiln but the deal fell apart but I still
have the manual. Glad to see it will go to good use.

Deborah J. Bassett-Maxwell
Kimball, MI
www.redmuddcreations.com

=20



-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of
Heisler-Schafer, Tamie
Sent: Wednesday, November 08, 2006 12:02 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: Cress FE29P Kiln

Hello:

I just bought an 20 year old Cress FE29P electric kiln but unfortunately
it came with no manual. When I contacted Cress they said they did not
have any back issues of the manual. So, I'm hoping someone out there
can tell me a few details about firing with this kiln. There are
setting for the firing speed (A, B, C, D - normal to low plus manual),
plus there is a thumbwheel dial which can be set from 1 to 10. I'd
really appreciate it if someone can give me some advice on setting the
dials for bisquing (cone 06) and glazing (cone 6). Thanks very much!
-Tamie=20

________________________________________________________________________
______
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.