shellac as resist #2

updated sat 14 oct 06

 

JoyceLee on fri 13 oct 06


Oops. What Marcia said was:


>If you go to http://www.vasefinder.com/vasefinder.nats.2006.home.html
>my vase is the second shown. I used the acrylic medium for resist and
>applied several layyers of colored slips and resist-washed them away.
>Polyurethane also has bad fumes. I try to avoid such toxins.
>Marcia Selsor
>http://marciaselsor.com
--------------------------------------------------------------------
Len wote the section that I quoted and attributed to
Marcia. I have used the method that he described which
worked well for me.

Joyce
In the Mojave