kiln cement recipe?

updated mon 19 jun 06

 

debbie entwistle on sun 18 jun 06


Hi

Does anyone know a recipe for kilm cement?

Our top loader's lid's steel band keeping the bricks under compression snapped and the bricks have cracked as a consequence.

Our pottery is on a small tropical island and it'd be cool not to have to fedex in kiln cement if I can make it myself!

Any suggestions appreciated!
Cheers,
Debbie


---------------------------------