Dan Dermer on thu 1 jun 06


Crista,
The glaze combination on the nested bowls is...
1. Smokey Blue (available from Clay Planet in San Jose, CA), base glaze,
dipped overall.
2. Sun Valley Rutile (widely avail formula) sprayed in a band a couple
inches below the rims, inside & out.
3. Copper Red (use your favorite), sprayed in a band a just under the rims
and overlapping the S.V. Rutile a little.

The copper red goes purplish because of the rutile glaze underneath it.
These are cone 10 R glazes on a white stoneware clay.

-Dan

p.s. another example of this combination on my web site, on the middle mug:

http://www.higherfirestudios.com/trio-of-mugs.JPG

Crista Nelson on thu 1 jun 06


In a message dated 6/1/2006 2:14:06 P.M. Central Daylight Time,
millennia-antica@EMAIL.COM writes:

http://photos.yahoo.com/dbdermer


Dan those pieces with that lavender blue purple glaze are wonderful, are you
willing to share the recipe??? if not I understand... Thanks....