search  current discussion  categories  forms - misc 

bead racks

updated wed 3 may 06

 

Lili Krakowski on tue 2 may 06


You do not need to go out and buy something costly....You can get soft brick
and cut it to size, and use Kanthal wire which can be bought at ceramic
supply houses.

You also can make up a refractory mix of kaolin and fine grog--lots or
recipes--- and shape to your need.

If already yet you are going to go to the trouble of making pendants, then
you should consider going to the trouble of making supports....

And. Quite amusing supports can be made out of a mix as above with three
little prongs of wire stuck in vertically, in a triangle, to support stuff.
Also you can embed short pieces of broken elements, in this mix, same
idea....


Lili Krakowski