Just wondering if anyone could help me in finding out what when wrong with my glaze. I just resently started working in low temps ( used to working cone 10) and am having glaze troubles. The glaze I started with was

Frit 3124 ......75.5
Neph Sy.......9.4
EPK.............9.4
Lithium.........3.8
Bentonite......1.9

and I've been using a low fire, bought boxed clay





---------------------------------
How low will we go? Check out Yahoo! Messengerís low PC-to-Phone call rates.

Donna Kat on mon 24 apr 06


On Fri, 21 Apr 2006 15:27:03 -0700, S. Morris wrote:

>Hi all,
> Just wondering if anyone could help me in finding out what when wrong
with my glaze. I just resently started working in low temps ( used to
working cone 10) and am having glaze troubles. The glaze I started with was
>
> Frit 3124 ......75.5
> Neph Sy.......9.4
> EPK.............9.4
> Lithium.........3.8
> Bentonite......1.9
>
> and I've been using a low fire, bought boxed clay
>

What temp (cone) are you firing to and what went wrong?