Guy Watson on wed 12 apr 06


I'm seeking a Saturated Iron Red cone 6 recipe for use in an oxidation
environment. If anyone wants to part with one I would appreciate it---Guy

Neal on wed 12 apr 06


Guy: I have had good results with the temoku
glaze recipe posted by C. Harris back in
March 1999. It's in the archives here:

http://tinyurl.com/jtvqj

I use it on Highwater's Red Rock and Red
Stone clays and fire it to cone 6 with a
scheduled firing down.

Neal O'Briant

__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

Nanci Mansfield on wed 12 apr 06


Neal, please forgive this beginner for asking a dumb question but, what is a scheduled firing down? Please ealborate.
Thanks,
Nanci

Neal wrote:
Guy: I have had good results with the temoku
glaze recipe posted by C. Harris back in
March 1999. It's in the archives here:

http://tinyurl.com/jtvqj

I use it on Highwater's Red Rock and Red
Stone clays and fire it to cone 6 with a
scheduled firing down.

Neal O'Briant

__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.



---------------------------------
Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+ countries) for 2/min or less.