does anyone know of a watermelon glaze - note

updated sat 8 apr 06

 

Janine LaMaie on fri 7 apr 06


Br. Llewellyn

My earlier reply didn't mention that the Clay Art Center Candy Red is
probably a glaze made with a cadmium inclusion stain. You need to test for
food safeness (with watermelon, of course!)

Regards,
Janine