mel jacobson on tue 14 mar 06


that is an old alfred porcelain.
probably 1960.
it has a great deal of ball clay, so it
actually throws ok. it is white...for sure.
sticks to any stoneware like stones. and easy
to make. four cups, four pounds, four tons each, add water.
jon britt subs neph sy for a bit lower temp.
good idea.
mel