Crista Nelson on sun 12 mar 06


Candy, The glossy black and the rutile green came off of DIY's website from
potter Bill Van Gilder: here is a link to that page:
_http://www.diynetwork.com/diy/crafts/article/0,2025,DIY_13786_2935033,00.html_
(http://www.diynetwork.com/diy/crafts/article/0,2025,DIY_13786_2935033,00.html) and the Nutmeg
and white satin matt came from an article in Ceramics Monthly by Richard
Busch: here is a link to that site:
_http://www.ceramicsmonthly.org/mustreads/busch.asp_ (http://www.ceramicsmonthly.org/mustreads/busch.asp) ...
I used the firing chart from John and Rons website to fire these in my
kiln....Thanks for the compliments.... I would really like to see those copper
reds you got...Good potting... Crista

candy murguia on tue 14 mar 06


Thank you very much for sharing! My kiln just died so im getting the
elements replaced, as soon as I get it back and get another firning done
I'll send you some pictures of the reds, I sold my last batch. If you want
the recipe let me know and I'll send it to you. It's a basic copper red,
reformulated down to cone 6, with the addition of 5% triple fine silicon
carbide to produce an artificial reduction in the electric kiln.

Candy


>From: Crista Nelson
>Reply-To: Clayart
>To: CLAYART@LSV.CERAMICS.ORG
>Subject: Glazes-Re: a few pictures of my cone 6 firing
>Date: Sun, 12 Mar 2006 23:20:51 EST
>
>Candy, The glossy black and the rutile green came off of DIY's website
>from
>potter Bill Van Gilder: here is a link to that page:
>_http://www.diynetwork.com/diy/crafts/article/0,2025,DIY_13786_2935033,00.html_
>(http://www.diynetwork.com/diy/crafts/article/0,2025,DIY_13786_2935033,00.html)
> and the Nutmeg
>and white satin matt came from an article in Ceramics Monthly by Richard
>Busch: here is a link to that site:
>_http://www.ceramicsmonthly.org/mustreads/busch.asp_
>(http://www.ceramicsmonthly.org/mustreads/busch.asp) ...
>I used the firing chart from John and Rons website to fire these in my
>kiln....Thanks for the compliments.... I would really like to see those
>copper
>reds you got...Good potting... Crista
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.

_________________________________________________________________
Express yourself instantly with MSN Messenger! Download today - it's FREE!
http://messenger.msn.click-url.com/go/onm00200471ave/direct/01/