I want to clarify my previous post on this topic. The drippy surface I
mentioned was of the raw glaze just after being dipped, not after being
fired. In fact, we fired them this weekend, and all surfaces came out
looking even and normal. No drips, runs or unevenness. We're very
happy as these were pots we were preparing for new jury slides.