fuzzy molds

updated mon 23 jan 06

 

Pat Logue on sun 22 jan 06


Hi folks
In my experience, the fuzzy molds are nothing more than a nuisance, as I
think was mentioned.
I switched to air purge dies and ceramical plaster awhile back (credit to
Deer Creek pottery for their on line tutorial) and dont recall having the
problem lately.May just be a coincidence. I can always purge all the
moisture if it becomes an issue.
Pat