Ivor and Olive Lewis on sun 22 jan 06
Dear Tom Yocky ,
I think many answers to your questions will be solved if you get hold of =
and read: R. Fournier, "Electric Kiln Construction for Potters". 1977 =
ISBN 0442301340
Chapter 6, Design and Calculation of Kiln Elements. p 61 sounds good =
reading to me.
By the way, reading other posts on your topic I suggest you make sure =
you understand and can apply "Ohm's Law" which is the relationship =
between the Power in Amperes to the Current or Potential Difference in =
Volts and the Resistance of you wire in Ohms. Fournier does cover this =
topic.
Best regards,
Ivor Lewis.