Hank Murrow on thu 19 jan 06


Dear Gary;

Here is a link for the borax bead tests......... lots more info at this
site!

http://webmineral.com/help/BoraxBead.shtml

Tell us what you find,

Hank
www.murrow.biz/hank

Gary Navarre on fri 20 jan 06


Well Crew, in "localities" I found a link, MINDAT.ORG, that a rock
hound/bat counter up here gave me some time ago. I'd found small kaolinite
deposits mentioned along the shore of Lake Superior but they are too small
for commercial mining and other minerals were more profitable. The color
chart is great start. Interesting that keying out mushrooms starts with the
color of the spore print, not that they are connected. The search is still on.

G in da U.P.