search  current discussion  categories  glazes - misc 

steven hill glaze

updated sun 8 jan 06

 

Tony Ferguson on fri 6 jan 06


Mike,

Yeah, that glaze is based on Tom's yellow crystal matt without the yellow iron oxide and subbing frit for the GB.

Tony

Mike Gordon wrote:
Steven Hill glaze handout has a "Strontium Crystal Magic " glaze, is
this similar to the crystal matt glaze Tony F. was referring too? He
handed it out at a workshop here in Walnut Creek, Ca. last summer. Mike
Gordon

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.




Tony Ferguson
...where the sky meets the lake...
Duluth, Minnesota
Artist, Educator, Web Meister
fergyart@yahoo.com
fergy@cpinternet.com
(218) 727-6339
http://www.aquariusartgallery.com
http://www.tonyferguson.net

---------------------------------
Yahoo! Photos
Ring in the New Year with Photo Calendars. Add photos, events, holidays, whatever.

Mike Gordon on fri 6 jan 06


Steven Hill glaze handout has a "Strontium Crystal Magic " glaze, is
this similar to the crystal matt glaze Tony F. was referring too? He
handed it out at a workshop here in Walnut Creek, Ca. last summer. Mike
Gordon