Hi Donna,

Just thought I would warn everyone - the honey glaze has a very low
expansion rate - it will be a problem on some clays - best to do some fit
testing before using it - particularly as a linner glaze - check carefully
with a magnifying glass to see any shivering.

RR


>////////////////////////////////////////////////////////////
> Honey
>
>Spodumene 3000
>Flint 2000
>Gerstley B 1400
>Talc 1300
>Dolomite 700
>EPK (Kaolin) 500
>Rutile 600
>can add Ganular Manganese O2* 100-500
>Bentonite flocculent add to water 1st 190
> 9500