search  current discussion  categories  kilns & firing - misc 

=?iso-8859-1?q?re:=20=a0=20=a0=20=a0=20converting=20kiln=20from=20?=

updated mon 31 oct 05

 

Brad Carter on sun 30 oct 05

=?ISO-8859-1?Q?Electric=20to=20Gas?=

Whatever you do, don't buy a conversion kit from Summit kilns in Florida. I
bought one of there kits and the burners burned inside the burner tubes.
Never got it to work properly. The company owner didn't want to help me
troubleshoot the thing, so it went to the dump.