Sam or Mary Yancy on tue 18 oct 05


Take a bat, glue on a floor sanding disc. put the sanding disc/bat on your wheel. run the wheel slowley and place the pot/foot in the center of the moving bat. Will grind evenly. Just be sure to get the grinding dust out of the wheel pan with a brush and shop vacume to ensure no contamination or hurting the wheel bearings. You could also use wet-or dry sandpaper and water on the sanding whee/bat for a smother finish. When Flat, tilt the potto 'round out" the edge. Works for me. Sam in Daly City.

Tony Ferguson wrote:
Hi,



I am wondering if someone has found the ultimate bottom of pot/foot ring grinding device that will grind it flat without chipping away the edges. I have a bench grinder and diamond disk on my 4" grinder and they work but I need something that works better. Parts of the foot will pluck or chip away sometimes and so if anyone has ideas, I'm all ears.



Tony Ferguson






Tony Ferguson
...where the sky meets the lake...
Duluth, Minnesota
Artist, Educator, Web Meister
fergyart@yahoo.com
fergy@cpinternet.com
(218) 727-6339
http://www.aquariusartgallery.com
http://www.tonyferguson.net

---------------------------------
Yahoo! Music Unlimited - Access over 1 million songs. Try it free.

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.