search  current discussion  categories  techniques - stains 

iron stains.....

updated sun 23 oct 05

 

Hank Murrow on mon 17 oct 05


What gets 'em out in the laundry?

thanks, Hank
www.murrow.biz/hank

Pat Stern on wed 19 oct 05


I put lemon juice on cloth and then put it in the sun.Works perfectly on white, don't know what it woulddo to colored cloth. Pat--- On Tue 10/18, Peter Coates < Okieclay@COX.NET > wrote:From: Peter Coates [mailto: Okieclay@COX.NET]To: CLAYART@LSV.CERAMICS.ORGDate: Tue, 18 Oct 2005 14:16:00 -0500Subject: Re: Iron stains.....We use "Whink" Rust Stain Remover - for all colorfast fabrics... workspretty damn well... peace out...Pete in Oklahellma----- Original Message -----From: "Hank Murrow" To: Sent: Monday, October 17, 2005 8:59 PMSubject: Iron stains.....> What gets 'em out in the laundry?>> thanks, Hank> www.murrow.biz/hank>> ______________________________________________________________________________> Send postings to clayart@lsv.ceramics.org>> You may look at the archives for the list or change your subscription> settings from http://www.ceramics.org/clayart/>> Moderator of the list is Mel Jacobson who may be reached at>
melpots@pclink.com.______________________________________________________________________________Send postings to clayart@lsv.ceramics.orgYou may look at the archives for the list or change your subscriptionsettings from http://www.ceramics.org/clayart/Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

Karin on wed 19 oct 05


http://www.redbgone.com/howtolaundry.html


Karin Hurt
www.laughingbearpottery.com

----- Original Message -----
From: "Vince Pitelka"
To:
Sent: Tuesday, October 18, 2005 5:30 PM
Subject: Re: Iron stains.....


> Hank asked:
>> What gets 'em out in the laundry?
>
> I think that Louis Katz had the right idea. I recommend an all-rust-red
> wardrobe.
> - Vince
>
> Vince Pitelka
> Appalachian Center for Craft, Tennessee Technological University
> Smithville TN 37166, 615/597-6801 x111
> vpitelka@dtccom.net, wpitelka@tntech.edu
> http://iweb.tntech.edu/wpitelka/
> http://www.tntech.edu/craftcenter/
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>

Rose on sat 22 oct 05


At 06:59 PM 10/17/2005 -0700, you wrote:
>What gets 'em out in the laundry?
>
>thanks, Hank


Iron out, CLR, both in the laundry or cleaning section of your local grocery
store.

Rose Downs


Terra Madre
www.terramadre.com
2517 Greenfield Acres
Princeton, TX 75407-9734
469-450-5480