Doug Robinson on mon 10 oct 05


Q: This recipe fires beautifully at cone 8;
can anyone help me convert the recipe for cone 6?


MSA MATT cone 9 for oxidation

Soda Spar 42
Ball Clay 4
Dolomite 8
Flint 20
Gerstley Borate 12
Talc 14
Superpax 12

Thanks!

--
Laura Burch
Laura Burch Pottery
www.lauraburchpottery.com
607-275-0997