Or multicolored, depending where you live.



I'm looking for interesting 1260C (ox) glazes (?around cone 8 - don't work in cones I'm afraid) that show marked colour changes with thickness. Emmanuel cooper's 'shocking pink' is a good example, it's brown (thin) royal blue(medium) and pink/red where thick. I have another that's green/blue/pink.



does anyone else have recipes with good, contrasting colours?



Fiona W.



---------------------------------