Carolina Clay Guild is sponsoring a 2 day workshop on glazes with John Britt
Oct. 8 & 9. Since it's 2 days, not 5, we'll have the tests fired. Tests
will include glazes and fusion tests at cones 04 Electric, 6 electric, 10 ox
and redux and raku. Cost is $75 for members and $100 for non-members
(membership is $15 so you may want to join and save a little). Location is