marianne kuiper milks on thu 15 sep 05


Sorry, but there is still a big difference between
well water and spring water. Completely different
source and composition.
Our water is great to drink. No smell, just fresh like
"water". However: we have a lot of copper (judge tub
stains) and other stuff. i want to have it tested by
PennState labs because I feel that it pesters my
glazes. Guess I wasn't clear before, but we do not
have "hard" water.
Marianne
PS The suggestion to find out and balance/adjust added
chemicals is only logical and I will try that after
results come in. Thanks!