search  current discussion  categories  techniques - slips 

linseed oil for slip trailing

updated sat 10 sep 05

 

Gunnar Rasmussen on fri 9 sep 05


I was reading about the red wing potters that they used linseed oil to mix
thear cobalt slip do any potters do the same today i have mixed a small
test and it goes on smooth on bisq or dry ware