search  current discussion  categories  kilns & firing - cones & controllers 

pyro cones bending weird

updated tue 2 aug 05

 

Bonnie Dodson on mon 1 aug 05


Does anyone know why I occasionally get my witness cones in my electric
kiln bending as usual but the very tip curl up slightly? This doesn't
happen all the time and has occured in 06 and 6 temps.