search  current discussion  categories  glazes - misc 

what a difference a glaze base recipe makes, la la la !!!

updated thu 9 jun 05

 

Maurice Weitman on tue 7 jun 05


At 8:37 PM -0400 on 6/7/05, Edouard Bastarache Inc. wrote:
>at C/9=BD redux, just to verify the influence of glaze bases
>on a same mixture of opacifier/colourant, I conducted an
>expirement

Salut, Edouard,

I can understand that the two glaze bases would=20
result in differences in fired appearance.

But I'm amazed by how the G2A1 base caused the=20
pot on the left to shrink so much more than the=20
one glazed with the Vino base. Must be all that=20
Barium, eh?

Regards,
Maurice

Edouard Bastarache Inc. on tue 7 jun 05


Hi all,=20

at C/9=BD redux, just to verify the influence of glaze bases=20
on a same mixture of opacifier/colourant, I conducted an
expirement
The results can be seen on Lee Love's blogspot :

http://claycraft.blogspot.com/


Later,



"Ils sont fous ces quebecois"
"They are insane these quebekers"
"Est=E1n locos estos quebequeses"
Edouard Bastarache
Irreductible Quebecois
Indomitable Quebeker
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
www.sorel-tracy.qc.ca/~edouardb/Welcome.html
http://perso.wanadoo.fr/smart2000/index.htm
http://www.digitalfire.com/education/toxicity/

Edouard Bastarache Inc. on wed 8 jun 05


Salut Maurice

"But I'm amazed by how the G2A1 base caused the
pot on the left to shrink so much more than the
one glazed with the Vino base. Must be all that
Barium, eh?
Regards,
Maurice"

Your sense of humour has not shrunk over time.(GRIN)



"Ils sont fous ces quebecois"
"They are insane these quebekers"
"Están locos estos quebequeses"
Edouard Bastarache
Irreductible Quebecois
Indomitable Quebeker
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
www.sorel-tracy.qc.ca/~edouardb/Welcome.html
http://perso.wanadoo.fr/smart2000/index.htm
http://www.digitalfire.com/education/toxicity/