search  current discussion  categories  glazes - traditional iron glazes 

shinos in oxidation???

updated sat 4 jun 05

 

Betty Burroughs on fri 3 jun 05


A friend of mine loves the look of shino glazes but has an electric kiln.
Does anyone have a recipe for a shino-like glaze at Cone 6 to 8 oxidation?
She will be grateful for any suggestions.

Betty Burroughs
Victoria, BC

David Gallagher on fri 3 jun 05


I could give you one formulated for Cone 8 reduction? my guess is it will tun out white/gray though. Let me know if you'd like it

Betty Burroughs wrote:A friend of mine loves the look of shino glazes but has an electric kiln.
Does anyone have a recipe for a shino-like glaze at Cone 6 to 8 oxidation?
She will be grateful for any suggestions.

Betty Burroughs
Victoria, BC

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.



---------------------------------
Discover Yahoo!
Get on-the-go sports scores, stock quotes, news & more. Check it out!