Cindy Hart on wed 1 jun 05


Hi all,

Has anyone had any experience with "Chamois Matte" glaze? It was bought by
a student of ours at Artist Junction in Florida. The name was previously
something else. She was told they changed the name but no ingredients.
However, she has had trouble with large pinholes, craters ever since. She
has tried soaking. Firing bisque higher. etc. Just wondering if anyone
else knows of this glaze and is having the same problem or has a solution.

Thanks in advance,