Dean Poole on tue 17 may 05

My brother use to have a glaze he called Honey. I know it had Albany slip
in it and was fluid at cone 10 he fired it in the bottom of his kiln
around cone 8. It was blue orange and cream in reduction. I think he got
it from Dr. Schumacher while in collage At UNC Greeley CO. Dose this ring
any bells with anyone. It may have come from somewhere else and I am just
wishfully remembering. Thanks for any help. I would get it from him but
when Albany went the way of extinction he got rid of the recipe.