website update - waterfall brown over bone

updated thu 28 apr 05

 

Bert Gibson on mon 25 apr 05


Wanted to let people who might be interested know that I have updated my =
website with some recent pieces. They include some Cone 10 and some Cone =
6 Waterfall brown pieces. Be sure and check the last piece with =
waterfall brown over bone. Got some nice and unusual color development.

Bert Gibson
http://home.comcast.net/~lazybpottery/

Veena Raghavan on tue 26 apr 05


Hi Bert,

I enjoyed my visit to your web site. Great work and very nice glazes. Love
the combinations at both cone 6 and in reduction.

Thanks for sharing with us.

Veena

In a message dated 4/26/2005 4:11:25 AM Eastern Daylight Time,
lazybbeefmaster@COMCAST.NET writes:
>
> Wanted to let people who might be interested know that I have updated my
> website with some recent pieces. They include some Cone 10 and some Cone 6
> Waterfall brown pieces. Be sure and check the last piece with waterfall brown over
> bone. Got some nice and unusual color development.

VeenaRaghavan@cs.com

Janet Moe on tue 26 apr 05


Bert,

Thanks for the photos. The glazes look great! What
kind of clays are you using?? Thanks!

Janet, enjoying the sunny weather on the West Coast of
British Columbia

______________________________________________________________________
Post your free ad now! http://personals.yahoo.ca

Bert Gibson on wed 27 apr 05


Thanks Janet. For the cone 10 I am using "White Stoneware" from Trinity
Ceramics here in Dallas. The cone 6 is "Cone 6 Stoneware" also from Trinity
Ceramics which when fired is a buff color.

Bert Gibson


----- Original Message -----
From: "Janet Moe"
To:
Sent: Tuesday, April 26, 2005 7:08 PM
Subject: Website update - Waterfall Brown over Bone


> Bert,
>
> Thanks for the photos. The glazes look great! What
> kind of clays are you using?? Thanks!
>
> Janet, enjoying the sunny weather on the West Coast of
> British Columbia
>
> ______________________________________________________________________
> Post your free ad now! http://personals.yahoo.ca
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.