BJ Clark | Stinking Desert Ceramics on thu 21 apr 05


Hello All,
I was wondering if anyone would like to share base glazes that they
use on dinnerware. I have one glaze that I use as a stable base that I
add oxides and colorants to to achieve different colors.
I use a grey stoneware (48-s from Mile Hi).
I'd be willing to share my recipe if others would like to share
their's with me.
Or, I could post to the list if lots of people are interested.

Anyone else have stable, durable, dinnerware type glazes they'd like to sha=
re?
Thanks,

--=20
BJ Clark
Stinking Desert Ceramics
bjclark@stinkingdesert.com
www.stinkingdesert.com

BJ Clark | Stinking Desert Ceramics on sun 24 apr 05


Sorry, I forgot to mention in my previous message that this is for
cone 10, reduction atmosphere.
Thanks to everyone that has email me so far!

--=20
BJ Clark
Stinking Desert Ceramics
bjclark@stinkingdesert.com
www.stinkingdesert.com