Brian O'Neill on wed 20 apr 05


All Clayarters responding to my pokey, under-insulated oval kiln, a
hearty THANK YOU!

For the curious, all electrical issues appear to be fine, the problem
lies in the design. It's 3" brick and probably should be 4" given the
size of the kiln. So now I will "swaddle" the kiln in fiber and ITC the
insides for starters.

Thanks again,
Brian