gordo on wed 30 mar 05


had that same trouble not so long ago and when torn down found that the =
plug above it had began to burn out afetr the electrical repairs had to =
use compressed air to clean the trash from inside the switch.works fine =
now. been lurking for while but i am still here . howdy mel.