bill edwards on thu 24 mar 05


If you are running a vent keep it running for the
entire firing until the kiln reaches it temperature.
(I see you say your not able to get there) The
warranty if I remember correctly is the vent shouldn't
be turned off until its in the cooling phase at 1000 F
or below.

If you like, send me more information or the group and
we all can take a shot in the dark on the temperature
issue. Someone may have already hit the mark since I
am late reading this.

Bill Edwards


> A quick question about using my Orton Vent on an
electric kiln. Is it
> normal to leave the vent on during the entire firing
to say, cone 6
glaze?
> I'm having difficulty reaching temp, getting within
100 degrees F,
but it
> just doesn't make it. I thought the vent was
supposed to be left on
<>