search  current discussion  categories  techniques - misc 

grinding angle for dolan tools

updated tue 8 mar 05

 

Ken Chin-Purcell on mon 7 mar 05


What angle should you grind (sharpen) a Dolan tool at? It looks like
the total angle of the edge is about 60 degrees, but I just wondered
if anyone knew for sure. Looks can be deceiving...

-- Ken Chin-Purcell
www.bungalowpottery.com