search  current discussion  categories  glazes - misc 

earthenwaqre glazes

updated sat 5 mar 05

 

Bob Masta on fri 4 mar 05


Kier:

"The Potter's Complete Book of Clay and Glazes", revised edition,
has 59 "soft stoneware" glazes for C/04. Some of these use lead,
but there are plenty of borosilicate glazes in there.

Best regards,

Bob Masta