search  current discussion  categories  glazes - misc 

=?iso-8859-1?q?re:=20=a0=20=a0=20=a0=20re:=20glaze=20test=20for=20?=

updated thu 24 feb 05

 

Richard Busch on wed 23 feb 05

=?ISO-8859-1?Q?"Red"=20Nutmeg,=20cone=206,=20ox.?=

It should be yellow ochre. I know, it's my recipe. -Richard