Arnold - I just received my cone charts you so gracefully sent me. Got FIVE copies so I can post one at Skyline collge. Arnold Thank you Very much. I will be sure to buy your products whenever I can. Peace!!!. Sam Yancy, Daly City, CA

Arnold Howard wrote:From: "jen"
>I am relatively new to using my kiln,(used it twice) and need some help
> understanding what clay firing temps mean. Which is hotter, 05 or 06?
------------

Cone numbers without the zero in front (1, 2, 3, 4, etc.): The higher the
number, the hotter the temperature.

Cone numbers with the zero (01, 02, 03, 04): The higher the number, the
cooler the temperature.

It might help if you mentally replace the zero in front of a cone number
with a minus sign. (i.e. 01 = -1, 04 = -4.)

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
arnoldhoward@att.net / www.paragonweb.com

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.