Mike Gordon on wed 22 dec 04

You'll have to excuse the late response to this thread but it just
dawned on me that I use my incense burner with stick and cone incense
all the time. It is a face with a large nose and tongue sticking out,
which catches the ash from the stick kind and a surface for the cone
kind. No Problem at all with thermal shock from the cones. They leave
black circles is all which gives the guy a real strange look with black
dots on his tongue. It was fired at cone o4. Mike Gordon