Vince Pitelka on mon 29 nov 04

Subject: melt down

----- Original Message -----
From: "Rogier Donker"
To:
Sent: Monday, November 29, 2004 8:04 AM
Subject: Date: Sun, 28 Nov 2004 08:35:31 -0600From: Carleen lord
Subject: melt down


> Carleen..:-)
> Remove all lava and hope that you can do so without demolishing the brick
> and elements.....easier said than done, especially in a hobby kiln. Costly
> too....if the melt down is really, really bad you may have to purchase a
> new
> kiln. As to cause? A bunch of possibilities: Kilnsitter out of adjustment,
> blow up in the kiln that obstructed the KSTA, etc. etc. Hit my web site
> under Kiln repair....
> http://www.donkerstudio.org you might find some answers there. You can
> always E mail me and I'll help you out if I can.
> Rogier Donker
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>